Incorporation of 2D/3D porous materials in 6FDA-DAM polyimide-based membranes with enhanced CO2-based separation performance and aging resistance
- Authors
- Kang, Dohyoung; Jee, Hobin; Kim, Changhyuk; Chae, Sukbyung; Kim, Sang-Joon; Lee, Seonki; Yoo, Keunje; Chae, Kyu-Jung; Lee, Jungmin; Kwon, Soonchul; Chuah, Chong Yang; Yang, Euntae
- Issue Date
- Oct-2025
- Publisher
- Institution of Chemical Engineers
- Keywords
- 6FDA-DAM; Gas separation; H-BN; Mixed-matrix membrane; NiHCF
- Citation
- Process Safety and Environmental Protection: Transactions of the Institution of Chemical Engineers, Part B, v.202
- Indexed
- SCIE
SCOPUS
- Journal Title
- Process Safety and Environmental Protection: Transactions of the Institution of Chemical Engineers, Part B
- Volume
- 202
- URI
- https://scholarworks.gnu.ac.kr/handle/sw.gnu/80105
- DOI
- 10.1016/j.psep.2025.107817
- ISSN
- 0957-5820
1744-3598
- Abstract
- 6FDA-DAM-based mixed-matrix membranes (MMMs) were created by simultaneously incorporating two-dimensional (2D) hexagonal boron nitride (h-BN) and three-dimensional (3D) porous nickel hexacyanoferrate (NiHCF) to alleviate the trade-off between permeability and selectivity, as well as physical aging in polymeric membranes. Each nanofiller played a complementary role: h-BN contributed to improving the mixed-gas selectivity, while NiHCF enhanced both permeability and selectivity. Experimental results showed that the CO₂ separation performance of the MMM with dual additives was moderately enhanced as compared to the pristine 6FDA-DAM membrane. Under the condition of 2 wt% h-BN and 5.5 wt% NiHCF, the CO₂ permeability increased by approximately 32.6 %, while the CO2/N2 selectivity increased by 9.5 %. Moreover, the performance degradation caused by physical aging after 15 months was partially mitigated. While the pristine 6FDA-DAM membrane showed a 64.3 % and 60.7 % decrease in CO₂ permeability and selectivity, respectively, MMM with 2 wt% h-BN and 5.5 wt% NiHCF exhibited lower degradation rates, which registered at 56.3 % and 56.7 %, respectively. These results suggest that the additives stabilize the pore structure of the polymer, thereby suppressing polymer chain rearrangement and loss of free volume.
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - 해양과학대학 > Department of Marine Environmental Engineering > Journal Articles
- 공학계열 > 해양환경공학과 > Journal Articles

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.