M-type Sr-Hexaferrite에서 MnCO3 첨가에 따른 소결 거동Sintering Behavior of M-type Sr-Hexaferrite by MnCO3 Addition
- Other Titles
- Sintering Behavior of M-type Sr-Hexaferrite by MnCO3 Addition
- Authors
- 정민석; 유창재; 조중영; 문경석
- Issue Date
- 2020
- Publisher
- 한국분말재료학회
- Keywords
- Grain growth; Sintering; Sr hexaferrite; Microstructure control; Permanent magnet
- Citation
- 한국분말재료학회지, v.27, no.2, pp.126 - 131
- Indexed
- KCI
- Journal Title
- 한국분말재료학회지
- Volume
- 27
- Number
- 2
- Start Page
- 126
- End Page
- 131
- URI
- https://scholarworks.bwise.kr/gnu/handle/sw.gnu/7902
- DOI
- 10.4150/KPMI.2020.27.2.126
- ISSN
- 2799-8525
- Abstract
- The grain growth behavior of M-type Sr hexaferrite (SrM) grains is investigated with the addition of MnCO3. First, the SrM powder is synthesized by a conventional solid-state reaction. The powder compacts of SrM are sintered at 1250oC for 2 h with various amounts of MnCO3 (0, 0.5, 1.0, and 4.0 mol%). There is no secondary solid phase in any of the sintered samples. Relative density increases when MnCO3 is added to the SrM. Obvious abnormal grain growth does not appear in any of the SrM samples with MnCO3. The average grain size increases when 0.5 mol% MnCO3 is added to the SrM. However, as the amount of MnCO3 increase to over 0.5 mol%, the average grain size decreases. These observations allow us to conclude that the growth of SrM grains is governed by the two-dimensional nucleation grain growth mechanism, and the critical driving force for the growth of a grain decreases as the amount of MnCO3 increases.
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - 공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.