Detailed Information

Cited 0 time in webofscience Cited 7 time in scopus
Metadata Downloads

Influence of stereoisomerism of epoxy hardeners on fracture toughness of carbon fiber/epoxy compositesInfluence of stereoisomerism of epoxy hardeners on fracture toughness of carbon fiber/epoxy composites

Other Titles
Influence of stereoisomerism of epoxy hardeners on fracture toughness of carbon fiber/epoxy composites
Authors
권동준이민규권웅이은수정의경
Issue Date
Oct-2019
Publisher
한국탄소학회
Keywords
Epoxy resin Carbon composites Polymer matrix composites Fracture toughness Epoxy hardener
Citation
Carbon Letters, v.29, no.5, pp 449 - 453
Pages
5
Indexed
SCIE
SCOPUS
KCI
Journal Title
Carbon Letters
Volume
29
Number
5
Start Page
449
End Page
453
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/75110
DOI
10.1007/s42823-019-00060-w
ISSN
1976-4251
2233-4998
Abstract
Interfacial adhesion between carbon fiber and epoxy resin mostly determine the mechanical properties of the carbon fiber/epoxy composites and the chemical structures of epoxy resin and hardener plays an important role. In this regard, stereoisomerism of epoxy hardeners, such as 3,3′ and 4,4′-DDS (diaminodiphenylsulfone), can have significant influence on the fracture toughness of the cured epoxy and related carbon fiber composites. Therefore, this study aims to investigate the influence of stereoisomerism of epoxy hardeners on fracture toughness of the carbon fiber/epoxy composites. Triglycidyl aminophenol (TGAP) are selected as epoxy resin and 3,3′- and 4,4′-DDS are selected as epoxy hardener. Wetting behaviors and fiber matrix adhesion of TGAP/DDS mixtures onto carbon fiber are investigated and fracture toughness (KIC) of TGAP/DDS mixtures are also investigated. Then, the mode II fracture toughness test of the carbon fiber/TGAP/DDS composites are carried out to investigate the influence of hardener stereoisomerism on fracture toughness of the resulting composites. Wetting and fiber matrix adhesion to carbon fiber of TGAP/3,3′-DDS was better than those of TGAP/4,4’-DDS and KIC of TGAP/3,3′-DDS was also better than that of TGAP/4,4′-DDS. As a result of the synergistic effect of better wetting, fiber matrix adhesion, and fracture toughness of TGAP/3,3′-DDS, the mode II fracture toughness of the carbon fiber/ TGAP/3,3’-DDS composites was almost twice of that of the carbon fiber/ TGAP/4,4′-DDS composites. Based on the results reported in this study, stereoisomerism of the epoxy hardeners can influence the fracture toughness of the resulting composites as well as that of the resin itself. In other words, only small difference, such as the spatial arrangement of the molecular structure of epoxy hardeners can cause huge difference in the mechanical properties of the resulting composites.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Kwon, Dong-Jun photo

Kwon, Dong-Jun
대학원 (나노신소재융합공학과)
Read more

Altmetrics

Total Views & Downloads

BROWSE