Microstructural Effects on J-Integral Fracture Toughness of Welded High-Mn Steels at 298 and 77 K
- Authors
- Park, Sangeun; Kayani, Saif Haider; Park, Eun Hye; Kim, Jung Gi; Kim, Sangshik; Sung, Hyokyung; Seol, Jae Bok
- Issue Date
- Feb-2023
- Publisher
- Verlag Stahleisen GmbH
- Keywords
- cryogenic temperatures; heat-affected zones; high-Mn steels; J-integral fracture toughnesses; weld metals
- Citation
- Steel Research International, v.94, no.2
- Indexed
- SCIE
SCOPUS
- Journal Title
- Steel Research International
- Volume
- 94
- Number
- 2
- URI
- https://scholarworks.gnu.ac.kr/handle/sw.gnu/2799
- DOI
- 10.1002/srin.202200259
- ISSN
- 1611-3683
1869-344X
- Abstract
- J-integral fracture toughness tests are conducted on welded high-Mn steels at room and cryogenic temperatures. The specimens are categorized into weld metal (WM) and heat-affected zone (HAZ) to consider the different microstructural effects. The microstructure of WM is composed of dendrites formed during solidification, while the microstructure of HAZ consists of coarsened grains from the welding process. Both specimens show twinning behavior after J-integral fracture toughness tests at 298 K and the superior K (JIc) fracture toughness of WM (389 MPa root m) due to the formation of plentiful twins at the crack tip. At 77 K, K (JIc) fracture toughness of HAZ (221 MPa root m) is lower than that of WM (264 MPa root m) due to different stacking fault energies (SFEs). Twinning still prevails in WM at 77 K, while epsilon-martensite is formed in HAZ by relatively low SFE. The interface between gamma-matrix and epsilon-martensite can act as a crack initiation site during the fracture toughness test, leading to the deterioration of J-integral fracture toughness in HAZ.
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - 공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.