소결온도에 따른 (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 세라믹스의 구조적, 전기적 특성open accessStructural and Electrical Properties of (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 Ceramics with Variation of Sintering Temperature

Other Titles
Structural and Electrical Properties of (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 Ceramics with Variation of Sintering Temperature
Authors
이태호이성갑여진호
Issue Date
2012
Publisher
한국전기전자재료학회
Keywords
Structural properties; NKN; Electromechanical coupling factor; Dielectric constant
Citation
전기전자재료학회논문지, v.25, no.7, pp 506 - 510
Pages
5
Indexed
KCI
Journal Title
전기전자재료학회논문지
Volume
25
Number
7
Start Page
506
End Page
510
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/22936
DOI
10.4313/JKEM.2012.25.7.506
ISSN
1226-7945
2288-3258
Abstract
본 실험에서는 (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 세라믹스를 일반 소성법을 이용해 제작하였다. (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 세라믹스를 소결온도에 따라 구조적 전기적 특성에 대해 조사하였다. 소결온도에 따른 X-선 회절 분석으로는 X-선 회절모양의 변화는 관찰되지 않았으며, 모든 시편은 우선 배향성과 Na 또는 K의 휘발에 기인한 2차상 등이 없는 다결정성의 유사 입방(pseudo-cubic) 페로브스카이트 결정구조를 나타내었다. 소결온도가 증가함에 따라 소결밀도가 증가하는 것을 알 수 있었고, 최댓값은 1,020℃에서 4.5g/cm3 값을 나타내었다. 소결온도가 1,020℃인 (Na0.465K0.465Bi0.07)(Nb0.93Ti0.07)O3-0.08MnO2 세라믹스의 평균 결정립 크기는 0.83 µm이다. 또한 전기기계결합계수와 유전상수, 유전손실값은 각각 0.252,741 그리고 0.043%이다.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Lee, Sung Gap photo

Lee, Sung Gap
대학원 (나노신소재융합공학과)
Read more

Altmetrics

Total Views & Downloads

BROWSE