Effect of the Zirconia Particle Size on the Compressive Strength of Reticulated Porous Zirconia-Toughened Aluminaopen access

Authors
Lee, Chae-YoungLee, SujinHa, Jang-HoonLee, JongmanSong, In-HyuckMoon, Kyoung-Seok
Issue Date
Mar-2022
Publisher
MDPI
Keywords
reticulated porous ZTA; optimized viscosity; rheological control; compressive strength
Citation
Applied Sciences-basel, v.12, no.5
Indexed
SCIE
SCOPUS
Journal Title
Applied Sciences-basel
Volume
12
Number
5
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/1568
DOI
10.3390/app12052316
ISSN
2076-3417
Abstract
Featured Application Ceramic Membranes. Reticulated porous ceramics have attracted researchers owing to the separation and collection properties of porous materials and the combined high thermal resistance and chemical stability of ceramics. Among various kinds of reticulated porous ceramics, we investigated the feasibility of using reticulated porous Zirconia-toughened Alumina as applications such as dielectric barriers, insulators, and filters with acceptable properties. An acceptable range of the compressive strength for reticulated porous ZTA applications is approximately 1 MPa. However, when the pore density of the reticulated porous ZTA specimen prepared using coarse zirconia was 60, maximum compressive strength of 1.63 MPa was obtained. To enhance the compressive strength of reticulated porous ZTA specimens, rheological control of the ZTA slurry is most important by optimizing the viscosity of the ZTA slurry, and the composition (average particle size, solid loading, organic binder, and thickener) of the ZTA slurry was controlled. The optimized processing conditions to enhance the compressive strength of reticulated porous ZTA specimens were determined. Consequently, we enhanced the compressive strength of the reticulated porous ZTA specimens from 0.37 MPa to 3.11 MPa by optimizing the ZTA slurry when the solid loading content, the pore density, the sintering temperature, the amount of PVA, and the amount of thickener were 66 wt.%, 60 PPI, 1600 degrees C, 2 wt.%, and 0.15 wt.%, respectively.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Moon, Kyoung Seok photo

Moon, Kyoung Seok
대학원 (나노신소재융합공학과)
Read more

Altmetrics

Total Views & Downloads

BROWSE