Detailed Information

Cited 11 time in webofscience Cited 11 time in scopus
Metadata Downloads

Synthesis and properties of bonding layer containing flexible and fluorinated moieties for hydrocarbon-based membrane electrode assemblies

Authors
Nam, Soo-WhanYu, Duk ManKim, Tae-HoLee, Jang YongNam, Sang YongHong, Young Taik
Issue Date
Jul-2016
Publisher
Pergamon Press Ltd.
Keywords
Polymer electrolyte membrane; Bonding layer; Membrane electrode assembly; Sulfonated poly(arylene ether sulfone); Decal transfer method
Citation
International Journal of Hydrogen Energy, v.41, no.25, pp 10884 - 10895
Pages
12
Indexed
SCI
SCIE
SCOPUS
Journal Title
International Journal of Hydrogen Energy
Volume
41
Number
25
Start Page
10884
End Page
10895
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/15376
DOI
10.1016/j.ijhydene.2016.04.174
ISSN
0360-3199
1879-3487
Abstract
For membrane electrode assemblies (MEAs) consisting of hydrocarbon proton exchange membranes (PEMs) and Nafion-coated catalysts, the interfacial incompatibility between the membrane and electrodes has been a constant issue because it can seriously deteriorate the performance and long term stability of the MEAs. In this study, new bonding materials based on sulfonated aromatic copolymers with flexible and partially fluorinated structures (SPE/F) were prepared and tested as a proton conductive bonding layer on the surface of the hydrocarbon PEMs to increase the adhesive force to the catalyst layer. The SPE/F copolymers were synthesized by polycondensation of sulfonated and non-sulfonated dihalide monomers with two dihydroxy monomers, 4,4'-dihydroxy diphenyl ether (DHDPE) and hexafluoro bisphenol A (HFB). The molar feed ratio of DHDPE to HFB was varied (10:0, 7:3, and 4:6) in order to evaluate the effect of the polymer structure on the physical, electrochemical, and adhesive properties. With an increase in the HFB ratio, the proton conductivity and dimensional change of the resulting polymers decreased due to the enhanced chain rigidity and lower ion exchange capacity. The maximum adhesive strength of the bonding layer was obtained using a DHDPE:HFB ratio of 7:3 (SPE/F-7/3). Finally, the MEA utilizing SPE/F-7/3 as the bonding layer exhibited higher performance in the initial unit cell test, as well as a reduced increase in resistance after the durability cycling test compared with pristine MEA without the bonding layer. (C) 2016 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Nam, Sang Yong photo

Nam, Sang Yong
대학원 (나노신소재융합공학과)
Read more

Altmetrics

Total Views & Downloads

BROWSE