The Chemical and Physical Properties of Steam-Exploded Wood at Different Temperatures and Times at the Same Severity as a Dietary Fiber Source
- Jung, Ji Young;
- Ha, Si Young;
- Goel, Akshat;
- Jung, Chaemi;
- Choi, Yang-Ho;
- ... Yang, Jae-Kyung
WEB OF SCIENCE
6SCOPUS
6초록
The chemical and physical properties of steam-exploded pine chips were analyzed by varying the temperature (190 degrees C to 230 degrees C) and time (1.5 min to 20.0 min) of steam explosion at the same severity factor (R-o), i.e., 4.0. Then, their potential as a dietary fiber source was evaluated. Overall, the chemical properties, e.g., solid recovery, cellulose, hemicellulose, and total dietary fiber content, showed a tendency to decrease as the temperature increased as well as an increasing lignin content. The physical properties, e.g., water-holding capacity, oil-holding capacity, and swelling capacity, showed decreased values in pine chips subjected to steam explosion at a temperature of 210 degrees C or greater. The chemical and physical properties of the steam-exploded pine chips, which were subjected to steam explosion at different temperatures and times at the selected R-o) considerably changed, starting at a temperature of 200 degrees C for 11.5 min. Even with the same severity factor, the steam-exploded pine chips at a temperature of 200 degrees C for 11.5 min showed the greatest improvement in the physical properties, i.e., water holding capacity (8.3 g/g), oil holding capacity (6.8 g/g), and swelling capacity (4.9 mL/g).
키워드
- 제목
- The Chemical and Physical Properties of Steam-Exploded Wood at Different Temperatures and Times at the Same Severity as a Dietary Fiber Source
- 저자
- Jung, Ji Young; Ha, Si Young; Goel, Akshat; Jung, Chaemi; Choi, Yang-Ho; Yang, Jae-Kyung
- 발행일
- 2022-05
- 유형
- Article
- 저널명
- BioResources
- 권
- 17
- 호
- 2
- 페이지
- 2129 ~ 2142
- 언어
- ENG
- 출판사
- North Carolina University
- 발행국가
- 미국
- 분량
- 14 페이지
- ISSN
- E 1930-2126
P 1930-2126