Lithium sulfur cells were prepared by composing with sulfur cathode (PEO)(6)LiBF4 polymer electrolyte and lithium anode. (PEO)(6)LiBF4 polymer electrolyte was prepared under three different mixing conditions: stirred polymer electrolyte (SPE), ball-milled polymer electrolyte (BPE) and ball-milled polymer electrolyte with 10 wt%Al2O3 (BCPE). The effects of ball milling and additive were investigated by discharge test according to depth of discharge. The initial discharge capacity of lithium sulfur cell using BCPE was 1670 mAh g(-1)-sulfur, which was better than those of SPE and BPE, and approximately equal to the theoretical capacity. The cycle performance of Li/(PEO)(6)LiBF4/S cell was remarkably improved by the addition of Al2O3. (C) 2007 Elsevier B.V. All rights reserved.

키워드

sulfur; polymer electrolyte; ball milling; lithium sulfur cell; Al2O3; BATTERY
제목
Electrochemical properties of lithium sulfur cells using PEO polymer electrolytes prepared under three different mixing conditions
저자
Jeong, S. S.; Lim, Yt.; Choi, Y. J.; Cho, G. B.; Kim, K. W.; Ahn, H. J.; Cho, K. K.
DOI
10.1016/j.jpowsour.2007.06.108
발행일
2007-12
유형
Article; Proceedings Paper
저널명
Journal of Power Sources
권
174
호
2
페이지
745 ~ 750