상세 보기
초록
Thermomechanical pulping process uses large amounts of energy, mostly electricity to run electrical facilities. Thermomechanical pulp (TMP) made from Pinus densiflora also has a big drawback that refining consumes 90 per cent of the total energy used in TMP process. This study explored to draw up a way to save refining energy through different thermal treatment at the stages of presteaming and refining. Presteaming temperature was 80℃, 100℃, and 120℃. After presteaming at each temperature, refining was carried out at 100℃, 120℃, and 140℃respectively. In a presteaming stage, steaming temperature over 120℃greatly contributed to the decrease of refining energy leading to earlier attainment of a target freeness, irrespective of refining temperature. In addition, NaOH treatment with presteaming enhanced better development of fiber properties during refining than presteaming without NaOH. High temperature refining at 140℃produced a high strength paper, and wood chips treated by alkali responded betterto refining than at over 120℃. Improved softening effect on wood chips led to the decrease in shives contents but it gave no effect on pitch contents of TMP.
키워드
- 제목
- 국내산 소나무로 제조되는 열기계펄프 제조 기술 최적화연구 (1) - 목재 칩의 전처리와 리파이닝 시 온도와 NaOH 처리의 효과 -
- 제목 (타언어)
- Optimization Technology of Thermomechanical Pulp Made from Pinus densiflora (I) - Effect of Temperature and NaOH at Presteaming and Refining -
- 저자
- 남혜경; 김철환; 이지영; 박형훈; 권솔; 조후승; 이경선
- 발행일
- 2015
- 저널명
- 펄프종이기술
- 권
- 47
- 호
- 1
- 페이지
- 35 ~ 44
- 언어
- KOR
- 출판사
- 한국펄프·종이공학회
- 발행국가
- 대한민국
- 분량
- 10 페이지
- ISSN
- P 0253-3200