강판상에 굴 패각을 이용한 탄산칼슘 피막의 형성

Formation of Calcareous Deposit on Steel Plate by using Waste Oyster Shell

초록

Enormous amount of waste oyster-shell (OS) has a major disposal problem in coastal regions. OSs have attracted much attention for recycling, because these are mainly composed of calcium carbonate with rare impurities. In this study, we demonstrate the calcareous deposit films on steel plate by using OSs on the basic of cathodic protection technique. The composition of the OSs was analyzed by wavelength dispersive X-ray fluorescence spectrometer. Carbon dioxide gas was pumped into distilled water to make carbonic acid solution for dissolution of OS. The calcareous deposit was characterized by second electron microscope (SEM), energy dispersive X-ray analysis (EDX) and X-ray diffraction. Corrosion rates were estimated by measurements of anodic polarization and immersion test. It is confirmed that calcareous deposits on steel plate are formed under all condition of cathodic protection by using waste OS from the SEM and EDX results. Calcareous deposits on steel by OS provide good corrosion resistance by acting as a barrier to oxygen supply to the steel surface.

키워드

Calcareous deposit films; Cathodic protection; Oyster shell; Corrosion resistance
제목
강판상에 굴 패각을 이용한 탄산칼슘 피막의 형성
제목 (타언어)
Formation of Calcareous Deposit on Steel Plate by using Waste Oyster Shell
저자
김범수; 권재성; 김연원; 이명훈; 양정현
DOI
10.5695/JKISE.2017.50.6.531
발행일
2017
저널명
한국표면공학회지
권
50
호
6
페이지
531 ~ 535