와이어 방전가공이 초경과 두랄루민 표면의 화학 조성에미치는 영향Effects of Wire EDM on the Chemical Composition of Cemented Carbide and Aluminum 7075 Surfaces

Other Titles
Effects of Wire EDM on the Chemical Composition of Cemented Carbide and Aluminum 7075 Surfaces
Authors
김수진
Issue Date
Jan-2024
Publisher
한국기계가공학회
Keywords
Wire EDM(와이어방전가공); EDM Surface(방전표면); Cemented Carbide(초경합금); Aluminum 7075(알루미늄7075); SEM(주사전자현미경); EDS(에너지분산분광법)
Citation
한국기계가공학회지, v.23, no.01, pp 51 - 59
Pages
9
Indexed
KCI
Journal Title
한국기계가공학회지
Volume
23
Number
01
Start Page
51
End Page
59
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/69856
DOI
10.14775/ksmpe.2024.23.1.051
ISSN
1598-6721
2288-0771
Abstract
The chemical composition of the wire electric discharge machining (WEDM) recasting layer must be analyzed, asit affects the surface properties of the product. This study examines the WEDM surfaces of cemented carbide(WC) and aluminum 7075 by (scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy(EDS). Up to 87% of the diameter of the WC cylinder is machined by a brass wire. However, cracks and fluidforces break the remaining 13%. The broken cross-section consists of 1- -㎛ sized WC grains bonded with cobaltmetal and without brass elements. Copper elements, which do not exist in WC materials, are then detected onthe convex spherical portion of the WC WEDM surface, and tungsten, which is the main component of thematerial, is observed on the lower surface. This indicates that some brass electrode particles that were removedby the spark adheres to the cemented carbide surface. The aluminum component is uniform, but theconcentration of the copper component is scattered irregularly. Therefore, some melted electrodes appear to beirregularly attached to the aluminum 7075 WEDM surface. The oxygen component is distributed more in theconvex than in the concave portion, which means that the convex portion of the aluminum is mainly oxidized toalumina. On the WEDM surface of the WC under a high melting point, 16.7 wt.% of zinc and 41.8 wt.% ofcopper, which were not detected prior to electric discharge machining, are detected. However, on the WEDMsurface of aluminum 7075 with a low melting point, increases of only 8.8 wt.% of zinc and 6.3 wt.% of copperwere observed.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > 기계항공우주공학부 > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Kim, Su Jin photo

Kim, Su Jin
대학원 (기계항공우주공학부)
Read more

Altmetrics

Total Views & Downloads

BROWSE