Detailed Information

Cited 0 time in webofscience Cited 5 time in scopus
Metadata Downloads

Characteristics of lanthanum silicates electrolyte for solid oxide fuel cells

Authors
Lee, D.-J.Lee, S.-G.Noh, H.-J.Jo, Y.-W.
Issue Date
2015
Publisher
Korean Institute of Electrical and Electronic Material Engineers
Keywords
La9.33(Si5V1)O26; Lanthanum silicate; Mixed-oxide method; SOFC
Citation
Transactions on Electrical and Electronic Materials, v.16, no.4, pp 194 - 197
Pages
4
Indexed
SCOPUS
KCI
Journal Title
Transactions on Electrical and Electronic Materials
Volume
16
Number
4
Start Page
194
End Page
197
URI
https://scholarworks.gnu.ac.kr/handle/sw.gnu/18461
DOI
10.4313/TEEM.2015.16.4.194
ISSN
1229-7607
2092-7592
Abstract
La9.33 (Si5 V1)O26 ceramics were fabricated by the mixed oxide method for solid oxide electrolytes. La9.33 (Si5 V1)O26 specimens showed the hexagonal, space group P63 or P63/m, and the unit cell volume increased when the sintering temperature increased. The specimen sintered at 1,400˚C showed the X-ray patterns of the homogeneous apatite single phase without the second phase, such as La2 SiO5 and SiO2. The specimen sintered at 1,400˚C showed the maximum sintered density of 4.93 g/cm3. When the sintering temperature increased, the electrical conductivities increased, the activation energy decreased and the values were 7.83×10-4 S/cm, 1.61 eV at 600˚C, respectively. ?2015, KIEEME. All rights reserved.
Files in This Item
There are no files associated with this item.
Appears in
Collections
공학계열 > Dept.of Materials Engineering and Convergence Technology > Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Altmetrics

Total Views & Downloads

BROWSE